Figure 3:

Surface microscopic photographs (50 μm) of AZ91 pieces after different pre-treatments: A) bare alloy, B) at 4 V for 10 min, C) at 5 V for 10 min, D) 7 V at 10 min, and E) 10 V at 10 min.